I dissect, inspect and crush the slugs in three Waxers or "Wax Slugs" to see what properties the three different compounds of wax have. All slugs were poured in the same manner with smoking hot wax and a heavy load of shot. I use Crayola Crayon wax, Gulf Canning/Candle wax and a Special Blend of my own.

Crayon wax is not just wax. In fact Paraffin is only part of the wax compound that includes wax enhancers and microcrystalline wax to give it a certain durability under pressure. It has fillers and additives and pigment to make it opaque and leave a mark on paper a certain way. It has a medium high melting point, higher than general purpose Paraffin. It is tackier than Candle wax. It congeals more rapidly than Candle wax and the working time between reheating is shorter Once heated and mixed with shot it crumbles easily, but clings to the pellets and cup. It is difficult to scrape or crush away all the wax. The addition of microcrystalline wax creates the durable tacky nature of crayon wax, the fillers and pigments make it less effective as a binding agent though.

Gulf wax, or a similar general purpose canning and candle wax has a relatively low melt point and congeal point making it easy to work with. Once heated to 130F or so it melts readily. Paraffin has a low flash point, and will smoke at somewhere around 175F. At this point the paraffin is volatile and the vapor can easily be ignited causing a rapid fire ball. The wax stays liquid for a long time after being heated to the smoking point. General purpose wax is fairly hard and brittle...it tends to flake or fracture when stressed out of shape. The bond between paraffin and plastic is weak and easy to break. The bond between lead shot and paraffin is a little stronger, but the wax only clings to the shot and cup until scraped or crushed and then it breaks away completely.

The Special Blend has a high melting point and will congeal fairly quickly as it cools. Like Candle wax it has a hard finish at room temperature, but it does not fracture easily and deforms when stressed out of shape before it breaks. It's gummy and slightly tacky more so than crayon wax. It clings to the shot cup and shot less than Crayon wax but more than Candle wax. It holds it's shape better under a crushing load.

Initial and rudimentary ballistic tests show:

Crayon wax makes a clean entry hole with progressively more ragged holes in the test medium, leaving crumbles of wax and  stray pellets of shot as well as a smear the color of the wax. When it stops it some shot tears past the final cavity, The final cavity was irregular in shape with several tears but had a central clump of wax and shot I estimate to be about 1/3 the total mass.

The Candle Wax slug stays makes a clean entry hole and stays together pretty well in the first half of the test medium. In the final cavity the pellets of shot were fairly condensed and there was a lump of wax and shot I estimate to be about 1/2 or a little more of the total mass;

The "Federal Burgundy" special blend wax tore neat holes almost all they way to the end of its trail through the test medium and held together well with the majority of the shot in a clump in the final cavity. Pellets did spray out into the surrounding cavity, but from my estimate about 2/3rds of the mass remained in a lump.

Penetration into the test medium was very similar for all 3 rounds and subsequent tests would be required to determine if shot placement or a particular load is skewing the results. But the "paper" trail an remaining material is still provided some useful data.

Stay tuned for the Ballistic Test video coming up soon :)