6. Crystal Cells magnesium core corrosion after 1 week
868 views · Published 15 March 2014 · 3:09 · Indexed 30 September 2026
Channel: Andy Shell · 2014 · Science & Technology
In this video I take apart 1 week old crystal cells made with Lasersaber's design & dead sea salts to show the corrosion occurring inside. I also compare crystal cells to just magnesium in water, distilled water & white vinegar. I would like to hear what you think about this stuff or what I'm possibly doing wrong. Crystal cells used: 3x 1/4" magnesium cores, 3/4" copper pipe & laser sabers crystal cell design @ 1.5" height 1/4" magnesium core, 3/4" copper pipe & dead sea salt from Ontario @ 1.25" height. (see 4. Crystal Cell video for details)
More from this channel
-
6:45
AudioSurf Faithless & The Prodigy - Insomnia Vs. Funky Shi
-
7:52
Review: Table desk shelves edge corner cushion baby safety bumper guard protector
-
7:42
1. Crystal Cell test with aluminium core
-
8:29
3. Crystal Cell magnesium core test designs with joule thief circuit
-
2:35
Review: Cell phone case & overall opinion of cell phone accessories from ebay china
-
8:04
4. Crystal Cells dead sea salts vs. Lasersaber design
-
5:42
5. Crystal Cells My series parallel clip & joule thief explained
-
6:10
7. Crystal Cells Corrosion testing of the jon cell